This search combines search strings from the content search (i.e. "Full Text", "Author", "Title", "Abstract", or "Keywords") with "Article Type" and "Publication Date Range" using the AND operator.
Beilstein J. Nanotechnol. 2018, 9, 1602–1612, doi:10.3762/bjnano.9.152
Figure 1: Scanning electron microscopy images of the anodic aluminum oxide (AAO) nanostructure on a sapphire ...
Figure 2: Atomic force microscopy measurements for samples (a–c) AAO60, (d–f) AAO70, and (g–i) AAO80.
Figure 3: Transmission electron microscopy measurements for sample AAO60 at different magnifications: (a) com...
Figure 4: Transmission electron microscopy measurements for sample AAO70 obtained at different magnifications...
Figure 5: Transmission electron microscopy measurements for AAO80 obtained at different magnifications: (a) c...
Figure 6: (a) Measured luminous wavelength versus energy and (b) luminous angle for samples AAO60, AAO70, AAO...
Figure 7: (a) Angle-resolved electroluminescence (AREL) spectra of samples FC-BLED and AAO70. Angular resolut...
Figure 8: Typical light output power–current–voltage (L–I–V) curves of the samples in this study.
Figure 9: Sample structure used in rigorous coupled-wave analysis (RCWA) calculations: (a) AAO sample structu...
Figure 10: Rigorous coupled-wave analysis (RCWA) results obtained with different Al2O3 thickness and air-hole ...
Figure 11: Rigorous coupled-wave analysis (RCWA) results with different Al thickness values and fixed Al2O3 th...
Figure 12: Structure of flip-chip LED with anodic aluminum oxide (AAO) processing.